MP35N Bright Bar

MP35N alloy steel bar is a nickel, chromium, cobalt alloy MP 35N is non-magnetic and possesses an ultra-high tensile strength, and provides for good ductility MP35N has a maximum 750 degree F temperature capability In addition, it has excellent corrosi

Delivery status: Hot-Rolled 、

Surface: Bright 、

Standard: AMS

Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other

Type: Photography

Keywords: MP35N MP-35N