KS NCF750 Enquiry | Print this page
KS NCF750 Details
Corrosion - resisting and heat - resisting superalloy plates and sheets
KS NCF750 Standard Download
Category | Type | Grade | Designations |
---|---|---|---|
Grades | Stainless Steels | NCF750 | Korea - KS , D 3531 (2007) | D 3532 (2002) | |
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 0.50 | ||
Mn | - | 1.00 | ||
P | - | 0.030 | ||
S | - | 0.015 | ||
Cr | 14.00 | 17.00 | ||
Ni | 70.00 | - | ||
Cu | - | 0.50 | ||
Al | 0.40 | 1.00 | ||
Ti | 2.25 | 2.75 | ||
Fe | 5.00 | 9.00 | ||
Nb+Ta | 0.70 | 1.20 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
239 (≥) | 316 (≥) | 31 | 44 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
252 (≥) | 967 (≥) | 11 | 21 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 113 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
195 | 876 | 564 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |
Grade | Standard | Country | Application |
---|---|---|---|
NCF750 | KS | Korea | Corrosion - resisting and heat - resisting superalloy plates and sheets |
NCF750 | CNS | China | CNS Standard heat resistant alloy and corrosion resistant alloy bar and plate type and chemical composition |